The Steel Encyclopedia:
Learn Quickly. Choose with Confidence.

Steel terminology, standard equivalents, surface finishes, and answers to common questions—all in one place.

Quick Glossary

Chromium · CrThe key element behind stainless behaviour; at least about 10.5% is needed to form a protective layer.
Nickel · NiStabilizes the austenitic structure and improves formability and toughness; it also has a major effect on price.
Molybdenum · MoImproves resistance to pitting and chlorides; found in 316 and Duplex grades.
L grade (low carbon) · LFor example, 316L. Lower carbon reduces the risk of intergranular corrosion after welding.
Passive layer · Passive layerA very thin chromium-oxide layer that protects the surface and reforms after minor scratches.
Pitting corrosion · PittingSmall, localized cavities, often caused by chlorides such as those in seawater.
Intergranular corrosion · IntergranularCorrosion along grain boundaries that may occur after welding or improper heat exposure.
PVD · PVDA thin coloured coating on sheet (gold, rose gold, or black), often used for decorative applications.
2B finish · 2BA standard matte-to-semi-bright finish on cold-rolled sheet; the most common industrial finish.
BA finish · BABright annealed: a smooth, bright surface with good reflectivity.
Hairline · HairlineA linear brushed finish (No. 4) with a satin appearance that tends to show fewer fingerprints.
Mirror polish · No.8A highly polished, mirror-like surface for façades and decorative use.
Tread plate · Checker plateSheet with raised patterns to improve slip resistance on floors and steps.
Angle and channel dimensions · B · H · tB is width, H is height, and t is section thickness.

No results found. Try another term.

Grade Guides

Grade Equivalents in Standards

Grade (AISI)European number (EN)Japanese equivalent (JIS)Family
3041.4301SUS304Austenitic
3161.4401SUS316Austenitic
316L1.4404SUS316LAustenitic
3211.4541SUS321Austenitic
4301.4016SUS430Ferritic
22051.4462—Duplex

Surface Finishes

Matte (2B)Bright (BA)Brushed (Hairline)Mirror (No. 8)Coloured PVDPatterned and tread plate

FAQs

What is the difference between 304 and 316?

316 contains molybdenum and offers greater resistance to chlorides, seawater, and chemicals. 304 is often adequate and more economical for general use.

Is stainless steel magnetic?

304 and 316 are usually non-magnetic, although forming and cold working can make them slightly magnetic. 430 and Duplex are magnetic, so a magnet test cannot identify a grade reliably.

Why can stainless steel rust?

Common causes include iron contamination, high chloride exposure, or damage to the protective layer. Proper cleaning and grade selection help reduce the risk.

Which grade is suitable for a marine environment?

316 or 316L; for more severe conditions, Duplex 1.4462 may be considered.

Where is tread plate used?

On floors, steps, and walkways where slip resistance is important.

Didn’t find your answer?

Contact Arta Steel Vira’s specialists for guidance on a suitable grade and product.

Request Advice and Pricing

The information above is general and approximate. For critical or technical projects, refer to the product specification and mill certificate.