Stainless Steel 321 / 310
Heat-resistant grades: 321 is stabilized with titanium, while 310 is designed for more severe heat.
AusteniticFamily
GoodCorrosion resistance
HighRelative price
Usually non-magneticMagnetism
Composition and Specifications
| Element | Approximate percentage |
|---|---|
| European number (EN) | 1.4541 / 1.4845 |
| 321 – Chromium / Nickel | 17–19% / 9–12% + titanium |
| 310 – Chromium / Nickel | 24–26% / 19–22% |
Key Features
Thermal stabilityHigh-temperature service
321: titanium stabilizedReduces intergranular corrosion at temperature
310: high chromium and nickelOxidation resistance at very high temperatures
WeldableSuitable for fabrication and repair
Applications
Furnaces and burnersHeat exchangersExhaust systemsSteam lines
Note: Confirm operating temperature and gas environment with a technical specialist before final selection.
Quick Comparison
Compared with 304: more stable at high temperatures, but more expensive.
Related Products
Stainless Steel SheetStainless steel pipeBar
FAQs
What is the difference between 321 and 310?
321 is suited to moderately high temperatures and welded service; 310 is used at much higher temperatures.
Why does 321 contain titanium?
To help prevent intergranular corrosion in a critical temperature range.
Request a stainless steel quote 321 / 310
Share the dimensions, thickness, and required quantity so Arta Steel Vira’s specialists can assist.
The information above is general and approximate. For critical or technical projects, refer to the product specification and mill certificate.